Oct 12, 2020 Leave a message

Cathode material for lithium battery capacity degradation

Lithium-ion batteries have the advantages of high volume energy density, high mass energy density, high working voltage, low self-discharge efficiency, and no memory effect, and have been widely used in consumer electronic products. With the continuous expansion of the application field of lithium-ion batteries, the performance requirements for lithium-ion batteries are getting higher and higher, which also poses new challenges to the field of lithium-ion batteries. The problems encountered in the use of lithium-ion batteries, such as faster capacity decay at high temperatures, poor rate performance, and high self-discharge rate, have restricted their applications.


Reducing the decay rate of lithium batteries is the main content of current research, commonly known as the service life of lithium batteries. The composition of lithium-ion batteries mainly includes four main parts: positive electrode, negative electrode, separator and electrolyte. The capacity of lithium ion batteries mainly depends on the quality and ratio of the positive and negative active materials. There are many factors affecting the cycle life of lithium-ion batteries, such as the compatibility of the positive and negative active materials with the electrolyte, the preparation process and composition of the active materials, the structural characteristics of the positive and negative electrodes, the purity and composition of the electrolyte, and the thermal stability of the separator Sex and chemical stability, etc.


Cathode materials are one of the key factors that determine the life of lithium batteries. Currently, the commonly used cathode materials for commercial lithium batteries include layered LiCoO2, spinel-like LiMn2O4, and olivine-like LFP. This article mainly talks about the relationship between the cathode material and the capacity decay of the battery, and does not cover the relationship between other materials and the capacity decay too much.

1

Lithium cobalt oxide battery attenuation

Lithium cobaltate has a layered structure, which can ensure the degree and reversibility of structural changes during the deintercalation and intercalation of Li+. The main reasons for the capacity degradation of lithium cobalt oxide batteries are as follows:


(1) Reduced active lithium ion


With the use of lithium batteries, the amount of active lithium ions in the internal electrolyte gradually decreases. At the same time, due to the decrease in the mass transfer capacity of lithium ions, the capacity of the lithium ion battery is also attenuated. The loss of active lithium ions is mainly caused by the continuous consumption of active lithium ions by the reaction between the electrolyte and the positive and negative active materials during the cycle. Some research data show that under a small number of cycles, although the positive electrode material does not undergo a phase change, the regularity of the layered structure of LiCoO2 is reduced, which leads to difficulties in the insertion and extraction of lithium ions, and reduces the output capacity of the lithium battery.


https://image.ipaiban.com/upload-ueditor-image-20171030-1509359572927076756.png


(2) The charge and discharge rate is too large and the structure changes


In the previous article, it was mentioned that the fast charging of mobile phones is a multiplier within a safe range, and the impact on the battery is very small, so I will re-explain it here. However, charging and discharging at high rates will also affect the service life of lithium batteries. The increase in discharge rate will result in the mixing of Li and Co atoms, causing part of LiCoO2 to change from hexagonal crystal to cubic crystal. The structure of the positive electrode material changes, leading to capacity degradation. .


(3) The impedance of the positive electrode increases and the capacity of the negative electrode decreases

             

In the study, T. Osaka et al. found the rule shown in the figure below. As the number of battery cycles increases, the impedance of the positive electrode increases significantly but the impedance of the negative electrode does not change significantly. At the same time, the negative electrode capacity is found to decrease sharply but the positive electrode capacity is not obvious. Variety. It can be concluded that the capacity decline of the battery during cycling is due to the increase of the positive electrode interface impedance and the loss of negative electrode capacity.


https://image.ipaiban.com/upload-ueditor-image-20171030-1509359589502091871.png


(4) The use temperature is too high


In addition, an excessively high use temperature (such as 50°C) will cause the battery to decay faster. Before a small number of cycles, the discharge capacity of the battery at high temperature is higher than the rated capacity of the battery and the capacity at room temperature. This is due to the electrolyte at high temperature. With low viscosity, fast ion mass transfer, and high reaction activity of the pole piece, the battery exhibits a higher charge and discharge capacity. However, as the number of cycles increases, the polarization of the battery becomes serious, and its capacity is prone to sudden decrease.


https://image.ipaiban.com/upload-ueditor-image-20171030-1509359608292013838.png

2

Lithium manganate battery attenuation

Lithium manganate has a spinel structure to meet the demand for lithium ion deintercalation. However, the Mn in this material easily dissolves into the electrolyte at high temperatures, causing irreversible capacity loss. In addition, when discharging at a higher temperature, the material is prone to Jahn-Teller effect, which destroys the crystal structure of the active material, resulting in faster battery capacity degradation.


https://image.ipaiban.com/upload-ueditor-image-20171030-1509359622912040415.png


The main reasons for the capacity degradation of lithium manganate batteries are as follows:


(1) The electrochemical reaction of the electrolyte under high voltage is generally higher than 4.0V;

(2) Irreversible phase transition and structural transformation, such as Jahn-Teller effect;

(3) Mn in LiMn2O4 material dissolves into the electrolyte, mainly due to the disproportionation reaction.


Among the above-mentioned factors, the most important is the dissolution of Mn. The main reason for this phenomenon is the presence of HF in the electrolyte. HF will accelerate the dissolution of Mn in LiMn2O4, leading to the destruction of the crystalline structure of the cathode material.


During the charging and discharging process, with the insertion and extraction of Li+, the lattice constant of LiMn2O4 changes, and a phase transition occurs between the cubic system and the tetragonal system. The diffusion rate of Li+ in the cathode material is lower than the intercalation rate of Li+ on its surface. When the potential is about 4V, Li+ is enriched on the surface of LiMn2O4, which leads to the Jahn-Teller effect


3

Lithium iron phosphate battery attenuation


LFP has an olivine-like structure with good stability and safety. The theoretical capacity reaches 170mAh/g. The main domestic battery and electric vehicle manufacturers are BYD. Under normal circumstances, there are many factors that affect battery capacity:


(1) The positive and negative side reactions lead to the reduction of recyclable lithium and the destruction of the balance between the positive and negative electrodes; (2) The loss of active materials, such as material dissolution, structural deterioration, particle segregation and electrode delamination .


The research on the attenuation of LFP batteries is also more in-depth. The high-temperature cycle capacity of commonly used graphite system power batteries decays quickly, mainly because Fe3+ in the positive electrode is dissolved and deposited on the surface of the anode, and further reduction occurs to generate Fe metal particles, leading to anode polarization increase.


M Kassem et al. found in the study of LiFePO4/graphite system batteries that storage temperature is the direct cause of capacity loss. At the same time, the state of charge of the battery also affects the rate of its capacity loss. The high storage temperature and SOC cause the loss of recyclable lithium ions. EIS analysis showed that the diffusion impedance increased slightly, the ohmic impedance (including electrolyte impedance, contact impedance, etc.) and electrochemical reaction impedance increased more, of which the electrochemical impedance increased the most. The capacity loss mainly comes from the side reaction of the electrode and the electrolyte, which is an irreversible capacity loss. The loss of active lithium is the main cause of the capacity loss. It is attributed to the deterioration of SEI due to the volume change of the negative electrode during the cycle.


Send Inquiry

whatsapp

skype

E-mail

Inquiry